Baling Galvanized Wire Size:1.8-3.66mm Zine:30g-70g Tensile Strength:880-1600Mpa Packing : Coil,Z2, Pallet , Spider zinc coating mm SIZE(g/㎡)Min. zinc coating A1B2 〉0.80-1.00150120 〉1.00-1.20180150 〉1.20-1.40200150 〉1.40-1.60220150 〉1.60-1.80220180 〉1.80-2.20240190 〉2.20-2.50260210 〉2.50-3.00275240 Common product quality problems: 1. Improper zinc coating leads to winding cracking, which may be caused by low acid concentration, poor surface treatment of raw materials, improper ammonium chloride concentration and defects of materials. 2. Uneven intensity and poor extension, due to uneven intensity of raw materials and annealing temperature. 3. The main reason for the excessive resistance of galvanized wire used for armored cable is the raw material. 4. Poor color on the surface of galvanized wire, bluish and yellow. Possible causes include excessive oil pouring from asbestos tongs used for swabbing, and lack of aluminum in the helicopter zinc pot. 5. Improper handling of the joints, excessive wire diameter and mixing phenomenon, mainly due to improper handling by workers.China Special Wire website:http://www.tjhuayuanwire.com/special-wire/
|